Patent application number | Description | Published |
20110257363 | METHOD FOR PREPARING POLYARYLENE SULFIDE - The present invention relates to a method for preparing polyarylene sulfide, in which the polyarylene sulfide is prepared by a polymerization reaction of reactants including a diiodo aromatic compound and a sulfur compound, the method including: further adding 0.01 to 10.0 wt. % of diphenyl disulfide with respect to the weight of the polyarylene sulfide to the reactants to form the polyarylene sulfide having a melting point of 265 to 320° C. | 10-20-2011 |
20110269879 | HIGH-STRENGTH POLYPHENYLENE SULFIDE/POLYETHYLENE TEREPHTHALATE BLEND RESIN COMPOSITION AND METHOD FOR PREPARING THE SAME - The present invention relates to a high-strength inflammable blend resin composition including a polyphenylene sulfide resin and a polyethylene terephthalate resin. More specifically, the resin composition of the present invention includes: a basic blend resin containing 10 to 80 wt. % of a polyphenylene sulfide resin, and 20 to 90 wt. % of a polyethylene terephthalate resin; and 0.1 to 20 parts by weight of a modified polystyrene or a styrene-based elastomer with respect to 100 parts by weight of the basic blend resin. | 11-03-2011 |
20110269935 | METHOD FOR PREPARING POLYARYLENE SULFIDE WITH REDUCED FREE IODINE CONTENT - The present invention relates to a method for preparing polyarylene sulfide with a reduced free iodine content. More specifically, the method for preparing polyarylene sulfide includes: (a) polymerizing reactants including a diiodo aromatic compound and a sulfur compound to form a polyarylene sulfide; and (b) maintaining the polyarylene sulfide product at 100 to 260° C. for heat-setting. The preparation method of the present invention effectively reduces the free iodine content of the polyarylene sulfide to prevent potential corrosion of facilities for the subsequent process and improves the properties of the polyarylene sulfide product such as thermal stability, so the method can be usefully applied to industrial fields in regard to the preparation of polyarylene sulfide. | 11-03-2011 |
20120302726 | METHOD FOR PREPARING POLYARYLENE SULFIDE HAVING REDUCED IODINE CONTENT - This disclosure relates to a method for preparing polyarylene sulfide having reduced iodine content while having excellent thermal stability, specifically to a method comprising polymerization reacting a composition comprising diiodide aromatic compounds, sulfur compounds, and a polymerization terminator. The preparation method may effectively reduce iodine content of polyarylene sulfide to prevent corrosion of post processing equipment, improve properties of polyarylene sulfide such as thermal stability, and the like, and thus, it may be usefully applied in the industrial field relating to preparation of polyarylene sulfide. | 11-29-2012 |
20120322971 | RECYCLABLE POLYARYLENE SULFIDE AND PREPARATION METHOD THEREOF - This disclosure relates to recyclable polyarylene sulfide that may exhibit and maintain excellent mechanical properties, particularly does not exhibit decrease in melt viscosity when it is molten, and thus, exhibit little deterioration of mechanical properties, and a method for preparing the same. | 12-20-2012 |
20120329983 | POLYARYLENE SULFIDE HAVING REDUCED OUTGASSING AND PREPARATION METHOD THEREOF - This disclosure relates to polyarylene sulfide that may exhibit excellent processability at low temperature, decrease outgassing and flash or burr generation, and thus may satisfactorily mold a product requiring high molding accuracy, and a method for preparing the same. Specifically, the polyarylene sulfide includes an arylene sulfide repeat unit and an arylene disulfide repeat unit, wherein the weight ratio of the arylene sulfide repeat unit:arylene disulfide repeat unit is 1:0.0001 to 1:0.05. | 12-27-2012 |
20120329984 | POLYARYLENE SULFIDE AND PREPARATION METHOD THEREOF - This disclosure relates to polyarylene sulfide that may exhibit and maintain excellent properties and a method for preparing the same, wherein the polyarylene sulfide is in the form of pellet of 2 to 10 mm size immediately after melt polymerization, and has residual solvent content of 300 ppm or less, based on the total weight of resin. | 12-27-2012 |
20130115438 | POLYARYLENE SULFIDE HAVING EXCELLENT PROCESSABILITY AND PREPARATION METHOD THEREOF - The present invention relates to polyarylene sulfide, in which a ratio of a peak area of a polymer chain of a second polyarylene sulfide having a lower molecular weight than the maximum peak molecular weight to a peak area of a polymer chain of a first polyarylene sulfide having a higher molecular weight than the maximum peak molecular weight is 1.3 or less in the molecular weight distribution of the polyarylene sulfide, as measured by gel permeation chromatography using polystyrene as a standard, and a preparation method thereof. This polyarylene sulfide exhibits excellent processability and generates no burrs (flashes) or the like, and can satisfactorily mold a product requiring high molding precision. | 05-09-2013 |
20140345453 | CYLINDER DEVICE HAVING IMPROVED WEAR RESISTANCE THROUGH OPTIMAL ARRANGEMENT OF FINE TEXTURES - There is provided a cylinder device having optimal arrangement of fine textures and optimal surface roughness capable of reducing wear of a cylinder bore side and a piston ring by processing fine textures in an optimal selection region of the cylinder bore side to improve lubrication characteristics between the piston ring and the cylinder bore side while reducing engine oil consumption by processing surface roughness of the cylinder bore side to an optimal status. | 11-27-2014 |
20140350215 | METHOD FOR PREPARING POLYARYLENE SULFIDE HAVING REDUCED IODINE CONTENT - This disclosure relates to a method for preparing polyarylene sulfide having reduced iodine content while having excellent thermal stability, specifically to a method comprising polymerization reacting a composition comprising diiodide aromatic compounds, sulfur compounds, and a polymerization terminator. The preparation method may effectively reduce iodine content of polyarylene sulfide to prevent corrosion of post processing equipment, improve properties of polyarylene sulfide such as thermal stability, and the like, and thus, it may be usefully applied in the industrial field relating to preparation of polyarylene sulfide. | 11-27-2014 |