Patent application number | Description | Published |
20110020989 | METHOD FOR FORMING MICROCRYSTALLINE SEMICONDUCTOR FILM AND METHOD FOR MANUFACTURING THIN FILM TRANSISTOR - A microcrystalline semiconductor film having a high crystallinity is formed. Further, a thin film transistor having preferable electric characteristics and high reliability and a display device including the thin film transistor are manufactured with high mass productivity. A step in which a deposition gas containing silicon or germanium is introduced at a first flow rate and a step in which the deposition gas containing silicon or germanium is introduced at a second flow rate are repeated while hydrogen is introduced at a fixed rate, so that the hydrogen and the deposition gas containing silicon or germanium are mixed, and a high-frequency power is supplied. Therefore, a microcrystalline semiconductor film is formed over a substrate. | 01-27-2011 |
20110053358 | METHOD FOR MANUFACTURING MICROCRYSTALLINE SEMICONDUCTOR FILM AND METHOD FOR MANUFACTURING SEMICONDUCTOR DEVICE - An object of one embodiment of the present invention is to provide a technique for manufacturing a dense crystalline semiconductor film (e.g., a microcrystalline semiconductor film) without a cavity between crystal grains. A plasma region is formed between a first electrode and a second electrode by supplying high-frequency power of 60 MHz or less to the first electrode under a condition where a pressure of a reactive gas in a reaction chamber of a plasma CVD apparatus is set to 450 Pa to 13332 Pa, and a distance between the first electrode and the second electrode of the plasma CVD apparatus is set to 1 mm to 20 mm; crystalline deposition precursors are formed in a gas phase including the plasma region; a crystal nucleus of 5 nm to 15 nm is formed by depositing the deposition precursors; and a microcrystalline semiconductor film is formed by growing a crystal from the crystal nucleus. | 03-03-2011 |
20120021570 | METHOD FOR FORMING MICROCRYSTALLINE SEMICONDUCTOR FILM AND METHOD FOR MANUFACTURING SEMICONDUCTOR DEVICE - A seed crystal including mixed phase grains having high crystallinity with a low grain density is formed under a first condition, and a microcrystalline semiconductor film is formed over the seed crystal under a second condition which allows the mixed phase grains in the seed crystal to grow to fill a space between the mixed phase grains. In the first condition, the flow rate of hydrogen is 50 times or greater and 1000 times or less that of a deposition gas containing silicon or germanium, and the pressure in a process chamber is greater than 1333 Pa and 13332 Pa or less. In the second condition, the flow rate of hydrogen is 100 times or greater and 2000 times or less that of a deposition gas containing silicon or germanium, and the pressure in the process chamber is 1333 Pa or greater and 13332 Pa or less. | 01-26-2012 |
20120208360 | METHOD FOR FORMING SEMICONDUCTOR FILM AND METHOD FOR MANUFACTURING SEMICONDUCTOR DEVICE - A microcrystalline semiconductor film is formed over a substrate using a plasma CVD apparatus which includes a reaction chamber in such a manner that a deposition gas and hydrogen are supplied to the reaction chamber in which the substrate is set between a first electrode and a second electrode; and plasma is generated in the reaction chamber by supplying high-frequency power to the first electrode. Note that the plasma density in a region overlapping with an end portion of the substrate in a region where the plasma is generated is set to be higher than that in a region which is positioned more on the inside than the region overlapping with the end portion of the substrate, so that the microcrystalline semiconductor film is formed over a region which is positioned more on the inside than the end portion of the substrate. | 08-16-2012 |
20120211809 | SEMICONDUCTOR DEVICE, MANUFACTURING METHOD THEREOF, AND ELECTRONIC APPLIANCE - Provided are a semiconductor device with less leakage current is reduced, a semiconductor device with both of high field effect mobility and low leakage current, an electronic appliance with low power consumption, and a manufacturing method of a semiconductor device in which leakage current can be reduced without an increase in the number of masks. The side surface of a semiconductor layer formed of a semiconductor film having high carrier mobility is not in contact with any of a source electrode and a drain electrode. Further, such a transistor structure is formed without an increase in the number of photomasks and can be applied to an electronic appliance. | 08-23-2012 |
20120304932 | METHOD FOR MANUFACTURING MICROCRYSTALLINE SEMICONDUCTOR FILM AND METHOD FOR MANUFACTURING SEMICONDUCTOR DEVICE - An object of the present invention is to provide a technique for manufacturing a dense crystalline semiconductor film without a cavity between crystal grains. A plasma region is formed between a first electrode and a second electrode by supplying high-frequency power of 60 MHz or less to the first electrode under a condition where a pressure of a reactive gas in a reaction chamber of a plasma CVD apparatus is set to 450 Pa to 13332 Pa, and a distance between the first electrode and the second electrode of the plasma CVD apparatus is set to 1 mm to 20 mm; crystalline deposition precursors are formed in a gas phase including the plasma region; a crystal nucleus of 5 nm to 15 nm is formed by depositing the deposition precursors; and a microcrystalline semiconductor film is formed by growing a crystal from the crystal nucleus. | 12-06-2012 |
20150053972 | SEMICONDUCTOR DEVICE - To give favorable electrical characteristics to a semiconductor device. To provide a semiconductor device in which a change in electrical characteristics is suppressed. To provide a highly reliable semiconductor device. The semiconductor device includes a first insulating layer; a second insulating layer including an opening portion, over the first insulating layer; a semiconductor layer over the first insulating layer; a source electrode and a drain electrode that are apart from each other in a region overlapping with the semiconductor layer; a gate electrode overlapping with the semiconductor layer; and a gate insulating layer between the semiconductor layer and the gate electrode. The first insulating layer includes oxide, and the opening portion of the second insulating layer is positioned inside the semiconductor layer when seen from a top surface side and at least part of the opening portion is provided to overlap with the gate electrode. | 02-26-2015 |
20150179810 | SEMICONDUCTOR DEVICE - A change in electrical characteristics is suppressed and reliability in a semiconductor device using a transistor including an oxide semiconductor is improved. The semiconductor device includes an oxide semiconductor film over an insulating surface, an antioxidant film over the insulating surface and the oxide semiconductor film, a pair of electrodes in contact with the antioxidant film, a gate insulating film over the pair of electrodes, and a gate electrode which is over the gate insulating film and overlaps with the oxide semiconductor film. In the antioxidant film, a width of a region overlapping with the pair of electrodes is longer than a width of a region not overlapping with the pair of electrodes. | 06-25-2015 |