Patent application number | Description | Published |
20110146782 | METHODS TO PATTERN DIFFUSION LAYERS IN SOLAR CELLS AND SOLAR CELLS MADE BY SUCH METHODS - Methods exploiting a Self Aligned Cell (SAC) architecture for doping purposes, use the architecture to direct the deposition and application of either a dopant or a diffusion retarder. Doping is provided in regions that will become metallization for conducting fingers. Dopant may be treated directly into metallization grooves. Or, diffusion retarder may be provided in non-groove locations, and dopant may be provided over some or all of the entire wafer surface. Dopant and metal automatically go where desired, and in register with each other. The SAC architecture also includes concave surfaces for light absorbing regions of a cell, to reduce reflection of light energy, which regions may also be treated with dopant in the concavities, to result in semiconductor emitter lines. Alternatively, diffusion retarder may be treated into the concavities, leaving upper tips of ridges between the concavities exposed, thereby subject to deeper doping. | 06-23-2011 |
20110247546 | Ribbon Crystal String for Increasing Wafer Yield - A ribbon crystal has a body with a width dimension, and string embedded within the body. The string has a generally elongated cross-sectional shape. This cross-section (of the string) has a generally longitudinal axis that diverges with the width dimension of the ribbon crystal body. | 10-13-2011 |
20110247549 | METHODS AND APPARATI FOR MAKING THIN SEMICONDUCTOR BODIES FROM MOLTEN MATERIAL - A pressure differential is applied across a mold sheet and a semiconductor (e.g. silicon) wafer is formed thereon. Relaxation of the pressure differential allows release of the wafer. The mold sheet may be cooler than the melt. Heat is extracted almost exclusively through the thickness of the forming wafer. The liquid and solid interface is substantially parallel to the mold sheet. The temperature of the solidifying body is substantially uniform across its width, resulting in low stresses and dislocation density and higher crystallographic quality. The mold sheet must allow flow of gas through it. The melt can be introduced to the sheet by: full area contact with the top of a melt; traversing a partial area contact of melt with the mold sheet, whether horizontal or vertical, or in between; and by dipping the mold into a melt. The grain size can be controlled by many means. | 10-13-2011 |
20120038031 | DISPENSING LIQUID CONTAINING MATERIAL TO PATTERNED SURFACES USING A DISPENSING TUBE - Materials that contain liquid are deposited into grooves upon a surface of a work piece, such as a silicon wafer to form a solar cell. Liquid can be dispensed into work piece paths, such as grooves under pressure through a dispensing tube. The tube mechanically tracks in the groove. The tube may be small and rest at the groove bottom, with the sidewalls providing restraint. Or it may be larger and ride on the top edges of the groove. A tracking feature, such as a protrusion, Non-circular cross-sections, molded-on protrusions and lobes also enhance tracking. The tube may be forced against the groove by spring or magnetic loading. Alignment guides, such as lead-in features may guide the tube into the groove. Restoring features along the path may restore a wayward tube. Many tubes may be used. Many work pieces can be treated in a line or on a drum. | 02-16-2012 |
20120067273 | METHODS FOR EFFICIENTLY MAKING THIN SEMICONDUCTOR BODIES FROM MOLTEN MATERIAL FOR SOLAR CELLS AND THE LIKE - A pressure differential is applied across a mold sheet and a semiconductor (e.g. silicon) wafer (e.g. for solar cell) is formed thereon. Relaxation of the pressure differential allows release of the wafer. The mold sheet may be cooler than the melt. Heat is extracted almost exclusively through the thickness of the forming wafer. The liquid and solid interface is substantially parallel to the mold sheet. The temperature of the solidifying body is substantially uniform across its width, resulting in low stresses and dislocation density and higher crystallographic quality. The mold sheet must allow flow of gas through it. The melt can be introduced to the sheet by: full area contact with the top of a melt; traversing a partial area contact of melt with the mold sheet, whether horizontal or vertical, or in between; and by dipping the mold into a melt. The grain size can be controlled by many means. | 03-22-2012 |
20130036967 | SELECTED METHODS FOR EFFICIENTLY MAKING THIN SEMICONDUCTOR BODIES FROM MOLTEN MATERIAL FOR SOLAR CELLS AND THE LIKE - A pressure differential is applied across a mold sheet and a semiconductor (e.g. silicon) wafer (e.g. for solar cell) is formed thereon. Relaxation of the pressure differential allows release of the wafer. The mold sheet may be cooler than the melt. Heat is extracted almost exclusively through the thickness of the forming wafer. The liquid and solid interface is substantially parallel to the mold sheet. The temperature of the solidifying body is substantially uniform across its width, resulting in low stresses and dislocation density and higher crystallographic quality. The mold sheet must allow flow of gas through it. The melt can be introduced to the sheet by: full area contact with the top of a melt; traversing a partial area contact of melt with the mold sheet, whether horizontal or vertical, or in between; and by dipping the mold into a melt. The grain size can be controlled by many means. | 02-14-2013 |
20140083349 | REMOVABLE THERMAL CONTROL FOR RIBBON CRYSTAL PULLING FURNACES - A ribbon crystal pulling furnace has a base insulation and a liner insulation removably connected to the base insulation. At least a portion of the liner insulation forms an interior for containing a crucible. | 03-27-2014 |
20140220171 | APPARATI FOR FABRICATING THIN SEMICONDUCTOR BODIES FROM MOLTEN MATERIAL - A pressure differential can be applied across a mold sheet and a semiconductor (e.g. silicon) wafer (e.g. for solar cell) is formed thereon. Relaxation of the pressure differential can allow release of the wafer. The mold sheet may be cooler than the melt. Heat is extracted through the thickness of the forming wafer. The temperature of the solidifying body is substantially uniform across its width, resulting in low stresses and dislocation density and higher crystallographic quality. The mold sheet can allow flow of gas through it. The melt can be introduced to the sheet by: full area contact with the top of a melt; traversing a partial area contact of melt with the mold sheet, whether horizontal or vertical, or in between; and by dipping the mold into a melt. The grain size can be controlled by many means. | 08-07-2014 |