Patent application number | Description | Published |
20090263112 | HEAT TREATMENT APPARATUS AND METHOD FOR HEATING SUBSTRATE BY LIGHT IRRADIATION - In light-irradiation heating with a total irradiation time of one second or less, two-stage irradiation is performed, including a first stage of light irradiation of a semiconductor wafer, which irradiation produces an output waveform that reaches a peak at a given emission output; and a second stage of supplemental light irradiation of the semiconductor wafer, which irradiation is started after the peak, producing an emission output smaller than the above given emission output. The emission output in the second stage is two thirds or less than the above given emission output at the peak. The first-stage light-irradiation time is between 0.1 and 10 milliseconds, and the second-stage light-irradiation time is 5 milliseconds or more. This allows the temperature of the semiconductor wafer even at a somewhat greater depth below the surface to be raised to some extent while allowing the surface temperature to be maintained at a generally constant processing temperature. | 10-22-2009 |
20090285568 | HEAT TREATMENT APPARATUS AND METHOD FOR HEATING SUBSTRATE BY PHOTO-IRRADIATION - In photo-irradiation heating with a total photo-irradiation time of one second or less, after initial photo-irradiation of a semiconductor wafer is performed while increasing an emission output to a target value, succeeding photo-irradiation of the semiconductor wafer is performed while maintaining the emission output within a range of plus or minus 20% from the target value. The photo-irradiation time for the initial photo-irradiation ranges from 0.1 to 10 milliseconds, and the photo-irradiation time for the succeeding photo-irradiation ranges from 5 milliseconds to less than one second. This allows the temperature of the semiconductor wafer even at a somewhat greater depth below the surface to be raised to some extent while allowing the surface temperature to be maintained at a generally constant processing temperature, thus achieving both the activation of implanted ions and the repair of introduced defects without any thermal damage to the semiconductor wafer. | 11-19-2009 |
20120057855 | Heat Treatment Apparatus Emitting Flash of Light - Flash lamps connected to short-pulse circuits and flash lamps connected to long-pulse circuits are alternately arranged in a line. The duration of light emission from the flash lamps connected to the long-pulse circuits is longer than the duration of light emission from the flash lamps connected to the short-pulse circuits. A superimposing of a flash of light with a high peak intensity from the flash lamps that emit light for a short time and a flash of light with a gentle peak from the flash lamps that emit light for a long time can increase the temperature of even a deep portion of a substrate to an activation temperature or more without heating a shallow portion near the substrate surface more than necessary. This achieves the activation of deep junctions without causing substrate warpage or cracking. | 03-08-2012 |
20120061374 | Heat Treatment Apparatus Emitting Flash of Light - Flash lamps connected to short-pulse circuits and flash lamps connected to long-pulse circuits are alternately arranged in a line. The duration of light emission from the flash lamps connected to the long-pulse circuits is longer than the duration of light emission from the flash lamps connected to the short-pulse circuits. A superimposing of a flash of light with a high peak intensity from the flash lamps that emit light for a short time and a flash of light with a gentle peak from the flash lamps that emit light for a long time can increase the temperature of even a deep portion of a substrate to an activation temperature or more without heating a shallow portion near the substrate surface more than necessary. This achieves the activation of deep junctions without causing substrate warpage or cracking. | 03-15-2012 |
20120063751 | Heat Treatment Apparatus Emitting Flash of Light - Flash lamps connected to short-pulse circuits and flash lamps connected to long-pulse circuits are alternately arranged in a line. The duration of light emission from the flash lamps connected to the long-pulse circuits is longer than the duration of light emission from the flash lamps connected to the short-pulse circuits. A superimposing of a flash of light with a high peak intensity from the flash lamps that emit light for a short time and a flash of light with a gentle peak from the flash lamps that emit light for a long time can increase the temperature of even a deep portion of a substrate to an activation temperature or more without heating a shallow portion near the substrate surface more than necessary. This achieves the activation of deep junctions without causing substrate warpage or cracking. | 03-15-2012 |
20120114316 | HEAT TREATMENT APPARATUS AND METHOD FOR HEATING SUBSTRATE BY LIGHT IRRADIATION - In light-irradiation heating with a total irradiation time of one second or less, two-stage irradiation is performed, including a first stage of light irradiation of a semiconductor wafer, which irradiation produces an output waveform that reaches a peak at a given emission output; and a second stage of supplemental light irradiation of the semiconductor wafer, which irradiation is started after the peak, producing an emission output smaller than the above given emission output. The emission output in the second stage is two thirds or less than the above given emission output at the peak. The first-stage light-irradiation time is between 0.1 and 10 milliseconds, and the second-stage light-irradiation time is 5 milliseconds or more. | 05-10-2012 |
20130043229 | HEAT TREATMENT APPARATUS AND METHOD FOR HEATING SUBSTRATE BY LIGHT IRRADIATION - In light-irradiation heating with a total irradiation time of one second or less, two-stage irradiation is performed, including a first stage of light irradiation of a semiconductor wafer, which irradiation produces an output waveform that reaches a peak at a given emission output; and a second stage of supplemental light irradiation of the semiconductor wafer, which irradiation is started after the peak, producing an emission output smaller than the above given emission output. The emission output in the second stage is two thirds or less than the above given emission output at the peak. The first-stage light-irradiation time is between 0.1 and 10 milliseconds, and the second-stage light-irradiation time is 5 milliseconds or more. This allows the temperature of the semiconductor wafer even at a somewhat greater depth below the surface to be raised to some extent while allowing the surface temperature to be maintained at a generally constant processing temperature. | 02-21-2013 |
20140162467 | HEAT TREATMENT APPARATUS EMITTING FLASH OF LIGHT - Flash lamps connected to short-pulse circuits and flash lamps connected to long-pulse circuits are alternately arranged in a line. The duration of light emission from the flash lamps connected to the long-pulse circuits is longer than the duration of light emission from the flash lamps connected to the short-pulse circuits. A superimposing of a flash of light with a high peak intensity from the flash lamps that emit light for a short time and a flash of light with a gentle peak from the flash lamps that emit light for a long time can increase the temperature of even a deep portion of a substrate to an activation temperature or more without heating a shallow portion near the substrate surface more than necessary. This achieves the activation of deep junctions without causing substrate warpage or cracking. | 06-12-2014 |