Patent application number | Description | Published |
20090197006 | Protected Air-Activated Organotin Catalysts for Polyurethane Synthesis and Processes Therefore - This invention relates to a protected organotin-based catalyst system for polyurethane synthesis that is useful in coatings applications. The catalyst has low activity in the absence of oxygen. When a coating mixture comprising the catalyst is sprayed and/or applied to a substrate as a thin film in air, the catalyst is activated. For solvent-based refinish systems comprising hydroxyl and isocyanate species at high solids levels, the catalyst system therefore provides extended viscosity stability, i.e., pot life. | 08-06-2009 |
20100136251 | Protected air-activated organotin catalysts for polyurethane synthesis and processes therefore - This invention relates to a protected organotin-based catalyst system for polyurethane synthesis that is useful in coatings applications. The catalyst has low activity in the absence of oxygen. When a coating mixture comprising the catalyst is sprayed and/or applied to a substrate as a thin film in air, the catalyst is activated. For solvent-based refinish systems comprising hydroxyl and isocyanate species at high solids levels, the catalyst system therefore provides extended viscosity stability, i.e., pot life. | 06-03-2010 |
20100213454 | PROCESS AND MATERIALS FOR MAKING CONTAINED LAYERS AND DEVICES MADE WITH SAME - There is provided a process for forming a contained second layer over a first layer. The process comprises forming the first layer having a first surface energy and then treating the first layer with a photocurable surface-active composition which is a fluorinated ester or fluorinated imide of an α,β-unsaturated polyacid; exposing the photocurable surface-active composition patternwise with radiation resulting in exposed areas and unexposed areas; developing the photocurable surface-active composition to remove the unexposed areas resulting in a first layer having untreated portions in the unexposed areas and treated portions in the exposed areas, where the treated portions have a second surface energy that is lower than the first surface energy; and forming the second layer on the untreated portions of the first layer. There is also provided an organic electronic device made by the process. | 08-26-2010 |
20110092076 | APPARATUS AND METHOD OF VAPOR COATING IN AN ELECTRONIC DEVICE - An apparatus and method for vapor phase deposition of a reactive surface area (RSA) material onto a substrate of an electronic device. The vapor phase deposition is conducted at ambient pressures in air, and provides capture of residual vapor to minimize environmental release of RSA and other constituents used in the processing. | 04-21-2011 |
20110147718 | ELECTROACTIVE COMPOSITION AND ELECTRONIC DEVICE MADE WITH THE COMPOSITION - There is provided an electroactive composition including: a deuterated first host material and an electroluminescent dopant material. The first host is a compound having Formula I: | 06-23-2011 |
20120187382 | ELECTRONIC DEVICES HAVING LONG LIFETIME - An organic light-emitting diode is provided having an anode, a cathode, and an organic active layer therebetween. The organic active layer includes a deuterated compound and the device has a calculated half-life at 1000 nits of at least 5000 hours. | 07-26-2012 |
20150014675 | BLUE LUMINESCENT COMPOUNDS - There is provided a compound having Formula I | 01-15-2015 |
20150236278 | BLUE LUMINESCENT COMPOUNDS - There is provided a compound having Formula II | 08-20-2015 |
20150243909 | BLUE LUMINESCENT COMPOUNDS - There is provided a compound having Formula II | 08-27-2015 |