Inventors list |
Assignees list |
Classification tree browser |
Top 100 Inventors |
Top 100 Assignees |
Frommeyer
Alex X. Frommeyer, Cold Spring, KY US
| Patent application number | Description | Published |
|---|---|---|
| 20110300506 | Endodontic File With Working Length Adjustment Scale - An endodontic file is provided for use during root canal therapy. The endodontic file has a handle, a blade, and a marker. The marker provides a working length adjustment scale that is integrated with the handle and the blade. After adjustment of the endodontic file to a desired working length, compared to the depth of a subject root canal, the marker is maintained in a substantially static position relative to the blade, which is itself stationary relative to the handle. The endodontic file reduces the chances of unintended complications during root canal therapy, for example if the blade were to penetrate into various tissues located in proximity to the root canal. | 12-08-2011 |
Andreas Frommeyer, Aalen DE
| Patent application number | Description | Published |
|---|---|---|
| 20080310029 | Method for Improving the Imaging Properties of a Projection Objective, and Such a Projection Objective - The invention relates to a method -for improving the imaging properties of a micro lithography projection objective ( | 12-18-2008 |
Andreas Frommeyer, Schwaebisch Gmuend DE
| Patent application number | Description | Published |
|---|---|---|
| 20100128367 | PROJECTION OBJECTIVE FOR A MICROLITHOGRAPHY APPARATUS AND METHOD - A projection objective for a microlithography apparatus with improved imaging properties is provided. A manipulator for a projection objective is provided. A microlithography apparatus including a projection objective of this type and/or a manipulator of this type is provided. A method for improving the imaging properties of a projection objective is provided. | 05-27-2010 |
| 20100290024 | METHOD FOR IMPROVING THE IMAGING PROPERTIES OF A PROJECTION OBJECTIVE, AND SUCH A PROJECTION OBJECTIVE - The invention relates to a method-for improving the imaging properties of a micro lithography projection objective, wherein the projection objective has a plurality of lenses between an object plane and an image plane, a first lens of the plurality of lenses being assigned a first manipulator (ml, Mn) for actively deforming the lens, the first lens being deformed for at least partially correcting an aberration, at least one second lens of the plurality of lenses furthermore being assigned at least one second manipulator, and the second lens being deformed in addition to the first lens. Furthermore, a method is described for selecting at least one lens of a plurality of lenses of a projection objective as actively deformable element, and a projection objective. | 11-18-2010 |
Astrid Frommeyer, Basel CH
| Patent application number | Description | Published |
|---|---|---|
| 20120070330 | HIGH-STRENGTH STEEL SHEET AND THE METHOD FOR PRODUCTION THEREFOR - A high-strength steel sheet comprises, by weight, not less than 0.25% and not more than 0.5% of C, not less than 4% and not more than 14% of Mn, not less than 6.5% and not more than 9.5% of Cr, and not less than 0.3% and not more than 3% of Si. The high-strength steel sheet satisfies the following formulas 1 and 2 and mainly consists of austenite, and the high-strength steel sheet has yield strength of not less than 1000 MPa and total elongation of not less than 20%. | 03-22-2012 |
Dennis Keith Frommeyer, Sadieville, KY US
| Patent application number | Description | Published |
|---|---|---|
| 20090208696 | Adjustable bush trimmings tarp - The Adjustable Bush Trimmings Tarp ( | 08-20-2009 |
Georg Frommeyer, Erkrath DE
| Patent application number | Description | Published |
|---|---|---|
| 20120070330 | HIGH-STRENGTH STEEL SHEET AND THE METHOD FOR PRODUCTION THEREFOR - A high-strength steel sheet comprises, by weight, not less than 0.25% and not more than 0.5% of C, not less than 4% and not more than 14% of Mn, not less than 6.5% and not more than 9.5% of Cr, and not less than 0.3% and not more than 3% of Si. The high-strength steel sheet satisfies the following formulas 1 and 2 and mainly consists of austenite, and the high-strength steel sheet has yield strength of not less than 1000 MPa and total elongation of not less than 20%. | 03-22-2012 |
Joerg Frommeyer, Wallenhorst DE
| Patent application number | Description | Published |
|---|---|---|
| 20110168453 | ROCK DRILL BIT - A rock drill bit comprising a shank fitted with a clamping end and a drilling tip at the end away from the clamping end, the drilling tip comprising at least three, preferably exactly three blades which are alar in topview, said blades each comprising at their top side a lip constituted by a leading chipping face and a trailing flank, the lips substantially converging onto each other within a central zone centered on the drill bit axis, characterized in that, in the central zone, a single lip—long lip—runs through the bit axis and comprises a commensurate overshoot segment extending beyond the bit axis. | 07-14-2011 |
Ursula Frommeyer, Erkrath DE
| Patent application number | Description | Published |
|---|---|---|
| 20120070330 | HIGH-STRENGTH STEEL SHEET AND THE METHOD FOR PRODUCTION THEREFOR - A high-strength steel sheet comprises, by weight, not less than 0.25% and not more than 0.5% of C, not less than 4% and not more than 14% of Mn, not less than 6.5% and not more than 9.5% of Cr, and not less than 0.3% and not more than 3% of Si. The high-strength steel sheet satisfies the following formulas 1 and 2 and mainly consists of austenite, and the high-strength steel sheet has yield strength of not less than 1000 MPa and total elongation of not less than 20%. | 03-22-2012 |