Abu-Sharkh
Basel F. Abu-Sharkh, Dhahran SA
Patent application number | Description | Published |
---|---|---|
20100124666 | Method of applying polyelectrolyte multilayer film for corrosion control - The method of applying a polyelectrolyte multilayer film for corrosion control involves chemical and/or electrochemical pretreatment of a metallic substrate for better adherence of the protective film to the substrate. The method includes anodically polarizing the substrate in a solution of an acid for a period from one second to five hundred seconds before multilayer deposition. The acid may be an inorganic acid, such as sulfuric acid, phosphoric acid, hydrochloric acid, nitric acid, etc., or an organic acid, such as oxalic acid, acetic acid, etc. The method may include abrading the substrate and rinsing the substrate with deionized water before polarizing the substrate, and applying the polyelectrolyte multilayers following pretreatment. | 05-20-2010 |
Basel Fathi Abu-Sharkh, Al-Khobar SA
Patent application number | Description | Published |
---|---|---|
20130039824 | METHOD OF PRODUCING SODA ASH AND CALCIUM CHLORIDE - The method of producing soda ash and calcium chloride provides an environmentally friendly method of producing soda ash and calcium chloride without the production of waste and hazardous byproducts. The method of producing soda ash and calcium chloride is initiated with a volume of brine, which is ammoniated with gaseous ammonia to form ammoniated brine. Limestone is heated to produce calcium oxide and carbon dioxide. The ammoniated brine is reacted with the carbon dioxide to produce sodium bicarbonate, ammonium chloride and a brine effluent. The sodium bicarbonate is then calcined and decomposed to produce soda ash and gaseous carbon dioxide. The calcium oxide is reacted with the ammonium chloride to produce calcium chloride, water and ammonia. The ammonia is recycled to be used in the initial step of ammoniating the brine. The water and the brine effluent are also recycled and used to provide the brine in the initial step. | 02-14-2013 |
Basel Fathi Abu-Sharkh, Dhahran SA
Patent application number | Description | Published |
---|---|---|
20130216467 | METHOD OF PRODUCING SODA ASH AND CALCIUM CHLORIDE - The method of producing soda ash and calcium chloride provides an environmentally friendly method of producing soda ash and calcium chloride without the production of waste and hazardous byproducts. The method of producing soda ash and calcium chloride is initiated with a volume of brine, which is ammoniated with gaseous ammonia to form ammoniated brine. Limestone is heated to produce calcium oxide and carbon dioxide. The ammoniated brine is reacted with the carbon dioxide to produce sodium bicarbonate, ammonium chloride and a brine effluent. The sodium bicarbonate is then calcined and decomposed to produce soda ash and gaseous carbon dioxide. The calcium oxide is reacted with the ammonium chloride to produce calcium chloride, water and ammonia. The ammonia is recycled to be used in the initial step of ammoniating the brine. The water and the brine effluent are also recycled and used to provide the brine in the initial step. | 08-22-2013 |