Class / Patent application number | Description | Number of patent applications / Date published |
524064000 | Asphaltene or maltene additive | 14 |
20090062435 | Tire with Component Containing Asphaltene - The present invention is directed to a pneumatic tire including at least one component, the at least component including a rubber composition, the rubber composition including 100 parts by weight of a diene based elastomer and from 1 to 20 parts by weight, per 100 parts by weight of elastomer (phr), of a solvent-extracted asphaltene. | 03-05-2009 |
20100076122 | MODIFIED ASPHALT BINDERS AND ASPHALT PAVING COMPOSITIONS - A method for forming a modified asphalt binder composition, the method comprising preparing a phosphorus pentasulfide-binder concentrate by introducing and mixing phosphorus pentasulfide and asphalt binder, where the phosphorus pentasulfide-binder concentrate includes greater than 0.5 parts by weight phosphorus pentasulfide per 100 parts by weight asphalt, preparing a polymer-binder concentrate by introducing and mixing polymer and asphalt binder, where the polymer-binder concentrate includes greater than 5 parts by weight polymer per 100 parts by weight asphalt, and introducing and mixing the phosphorus pentasulfide-binder concentrate with the polymer-binder concentrate to form a modified asphalt binder composition, where the phosphorus pentasulfide includes a blend of P | 03-25-2010 |
20100076123 | MODIFIED ASPHALT BINDERS AND ASPHALT PAVING COMPOSITIONS - A method for forming a modified asphalt binder composition, the method comprising preparing a phosphorus pentasulfide-binder concentrate by introducing and mixing phosphorus pentasulfide and asphalt binder, where the phosphorus pentasulfide-binder concentrate includes greater than 0.5 parts by weight phosphorus pentasulfide per 100 parts by weight asphalt, preparing a polymer-binder concentrate by introducing and mixing polymer and asphalt binder, where the polymer-binder concentrate includes greater than 5 parts by weight polymer per 100 parts by weight asphalt, and introducing and mixing the phosphorus pentasulfide-binder concentrate with the polymer-binder concentrate to form a modified asphalt binder composition. | 03-25-2010 |
20110112225 | COMPOSITION AND A PROCESS THEREOF - The present invention provides solution to the problems involved in construction of roads which are economical and which have longer life and low maintenance requirement. It provides a crack free, skid resistant and ravel free road. Also, the invention provides a process for the construction of road which is capable of addressing the problems of prior art. | 05-12-2011 |
20110166266 | Composition for Sealing Joints in Road Surfaces and Subsurfaces - A composition that may be used to seal and strengthen the joints in an asphalt road surface and subsurface to prolong the useful life of the road is disclosed herein. The composition utilizes a polymer modified cationic maltene emulsion containing polymer modified maltene oils and resins, and surfactants/and wetting agents. The emulsion is applied to the longitudinal joints and other joints in the asphalt pavement surface. The emulsion reduces voids in the asphalt pavement and chemically improves the asphalt binder properties, thereby altering the modulus of elasticity of the asphalt binders so that the resistance of the pavement to tension is increased, and the water absorption of the pavement is reduced. | 07-07-2011 |
20120157583 | Roofing Granules, Roofing Products Including Such Granules, and Process for Preparing Same - A coating composition including an inorganic sol material and an organic colorant is applied to mineral particles and cured at a temperature less than 200 degrees Celsius. | 06-21-2012 |
20120225979 | ASPHALT MODIFIERS, METHODS OF MODIFYING ASPHALT, ASPHALT COMPOSITIONS AND METHODS OF MAKING - Asphalt compositions and products comprising petroleum asphalt, polyolefin, and a wax. | 09-06-2012 |
20120302673 | PREPARATION OF INDUSTRIAL ASPHALT - The present invention relates to a method for preparing an industrial asphalt comprising sparging an oxygen containing gas through an asphalt flux in the presence of 0.25 weight percent to about 12 weight percent of a highly saturated rubbery polymer at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt flux to a value which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm to produce the industrial asphalt. The highly saturated rubbery polymer can be a styrene-ethylene/butylene-styrene block copolymer rubber or a highly saturated styrene-ethylene/propylene-styrene block copolymer rubber. | 11-29-2012 |
20150080505 | PRE-SWELLED GROUND TIRE RUBBER AND METHODS OF MAKING AND USING THE SAME - Disclosed herein are compositions and methods relating to rubber compositions, comprising crumb rubber and a maltene-like oil, which provides simultaneous rut, crack, moisture, and temperature resistance in both dense grade and gap grade paving mixtures. Also disclosed are methods of producing the rubber compositions, and methods of using the same. | 03-19-2015 |
20150322316 | SYNTHETIC RAW ELASTOMERIC COMPOSITIONS IN FREE-FLOWING PELLET FORM AND PROCESS FOR OBTAINING THE SAME - A raw elastomeric composition in free-flowing pellet form is described, which comprises a raw elastomer with molecular weight from 50,000 to 400,000 Da, and an anti-block agent comprising inorganic fillers, capable of forming emulsions in water. Likewise, a process for obtaining said raw elastomeric compositions in free-flowing pellet form, comprising the steps of: a) polymerizing at least one monomer through solution polymerization in order to obtain elastomer crumb; b) forming an aqueous suspension of the elastomer crumbs; c) dewatering the aqueous suspension; d) adding an anti-block agent comprising inorganic fillers capable of forming emulsions in water; e) drying the dewatered suspension; and f) pelletizing the elastomer to form a raw elastomeric composition in free-flowing pellets form. The raw elastomeric composition in free-flowing pellets form thus obtained can be used as an adhesive composition, in asphalt modification and in asphalt emulsions. | 11-12-2015 |
20160017139 | Additive Composition for Polymer-Modified Asphalt, Polymer-Modified Asphalt Composition Comprising the Same, and Method for Preparing the Same - One aspect of the present invention provides an additive composition for polymer-modified asphalt including a block copolymer having a radial structure and a copolymer of an aromatic vinyl compound of which two ends have different molecular weights and a conjugated diene compound, and a method of preparing the same. When asphalt is prepared using the additive composition for polymer-modified asphalt, properties of the existing polymer-modified asphalt may be maintained while content of sulfur may be reduced, viscosity may decrease, and thereby processability and pavement performance may be improved. | 01-21-2016 |
20160017148 | ASPHALT COMPOSITIONS FOR ROOFING APPLICATIONS, METHODS FOR MAKING THE SAME, AND FILLED ASPHALT MATERIAL COMPRISING THE SAME - Asphalt compositions for roofing applications are provided, as well as filled asphalt material comprising the asphalt compositions and methods for making asphalt compositions and filled asphalt material. More particularly, the asphalt compositions comprise non-oxidized base asphalt; and a low molecular weight polyolefin present in an amount of from about 0.5 to about 15 wt % based on the total weight of the asphalt composition. The asphalt composition has a softening point from about 87.8 to about 160° C. (about 190 to about 320° F.), a penetration of greater than 12 deci-millimeters @ 25° C., as well as improved stain resistance and heat resistance. | 01-21-2016 |
20160017149 | PROCESS FOR THE PRODUCTION OF POLYMER MODIFIED BITUMEN USING NITROGEN RICH POLYCYCLIC AROMATIC HYDROCARBON - The present invention relates to a polymer modified bitumen composition comprising a petroleum vacuum residue, a nitrogen rich polycyclic aromatic hydrocarbon and a functionalized polymer having enhanced softening point, good antistripping effect, enhanced elastic recovery higher performance grade and low temperature creep stiffness effect. The present invention also relates to processes for the preparation of polymer modified bitumen composition. | 01-21-2016 |
20160032541 | Pot Hole Filler Composition and Method of Making Same - A system and method for filling pot holes. The system includes transferring aggregate from an aggregate tank. Activator is likewise transferred from an activator tank. The activator is mixed with the aggregate to form a homogenized mixture. A liquid is introduced into a homogenized mixture to form a slurry and then a pot hole filler. The pot hole filler is directed through an exit end of a mixing tube. | 02-04-2016 |