20080226396 | Seamless steel tube for use as a steel catenary riser in the touch down zone - The present invention describes an upset SCR of novel low carbon chemical composition and microstructure as well as method of manufacturing the same, which achieves higher improvement in the fatigue life as it is integral with the riser pipe section at the Touch Down Zone. The low carbon upset SCR achieves its desired properties by the thermal treatment which it is subjected to. The novel low carbon chemical composition and microstructure comprises in weight per cent, carbon 0.04-0.10, manganese 0.40-0.70, silicon 0.15-0.35, chromium 0.40-0.70, molybdenum 0.40-0.70, nickel 0.10-0.40, nitrogen 0.008 max, aluminum 0.010-0.045, sulfur 0.005 max, phosphorus 0.020 max, titanium 0.003-0.020, niobium 0.020-0.035, vanadium no more than 0.10, copper 0.20 max, tin 0.020 max, and carbon equivalent 0.43 max and PCM no more than 0.23 and having a yield strength of at least of 65000 psi, the ultimate tensile strength of at least 77000 psi and YS/UTS ratio below 0.89 in material representing the pipe body, the transition zone and the upset end. | 09-18-2008 |