| 20100221139 | Steel Having High Mechanical Strength and Wear Resistance - Method for reducing the segregated seams of a steel which has high mechanical strength and high wear resistance and whose composition comprises by weight: 0.30%≦C≦1.42%; 0.05%≦Si≦1.5%; Mn≦1.95%; Ni≦2.9%; 1.1%≦Cr≦7.9%; 0.61%≦Mo≦4.4%; optionally V≦1.45%, Nb≦1.45%, Ta≦1.45% and V+Nb/2+Ta/4≦1.45%; less than 0.1% of boron, less than 0.19% of (S+Se/2+Te/4), less than 0.01% of calcium, less than 0.5% of rare earths, less than 1% of aluminum, less than 1% of copper; the balance being iron and impurities resulting from the production operation. The composition further complies with: 800≦D≦1150 with D=540(C) | 09-02-2010 |