| EMS-CHEMIE AG Patent applications |
| Patent application number | Title | Published |
| 20110298152 | Thermoplastic Fiber Material Spun from a Raw Material Containing Polyhydroxyether, Methods for Its Production and Uses for It - The invention describes a new synthetic fiber material of polyhydroxyether, as well as a melt-spinning method for its production. The new material can be used, in particular, for stabilization of the reinforcement fibers of high-performance fiber composite materials before they are embedded in the matrix material. During this usage, the polyhydroxyether fiber material dissolves at a temperature above its glass transition temperature entirely in the matrix material, so that the reinforcement fibers can be arranged largely free of kinking. In addition, it forms cross-links with the matrix material to form a homogeneous matrix and thus does not constitute a disruptive third phase in the composite material. The compatibility of the matrix and reinforcement fiber is also improved. It was possible to improve the bending strength of test slabs by 12% as compared to that of reference slabs with polyester filament. | 12-08-2011 |
| 20110293868 | THERMOPLASTIC POLYAMIDE MOULDING COMPOSITIONS - The invention relates to thermoplastic polyamide moulding compositions containing: (A) at least 20% by wt. polyamide and/or at least one copolymer containing at least 20% by wt. polyamide structural units; (B) 0.01% by wt. to 2% by wt., relative to the polyamide portion and/or the portion of polyamide structural units, of the composition of a copper-containing stabiliser; and (C) 0.01% by wt. to 3% by wt., relative to the polyamide portion and/or the portion of polyamide structural units of the composition, of at least one organic compound containing metal complexing groups, so that the copper ions are present in complexed form through binding to the metal-complexing groups. These moulding compositions may be used as coating material for coolant lines. | 12-01-2011 |
| 20110240930 | POLYAMIDE MOLDING MATERIALS REINFORCED WITH GLASS FIBERS AND INJECTION MOLDED PARTS THEREOF - The present invention relates to reinforced polyamide molding materials with high notch impact strengths, comprising low viscous polyamides and flat glass fibers as a reinforcing medium, characterized in a polyamide matrix, comprising the following components: (A) 0 to 60 wt.-% of at least one aliphatic, partly crystalline polyamide with a solution viscosity, measured in m-cresol (0.5 wt-%), of η | 10-06-2011 |
| 20110217495 | POLYAMIDE MOULDING MATERIALS FOR THE PRODUCTION OF MOULDED ARTICLES HAVING REDUCED SURFACE CARBONIZATION - Moulded articles having reduced surface carbonization and longer retention of the mechanical properties and methods of producing same are presented. In an embodiment, the moulded article comprises polyamides with nanofillers, which can be produced by means of injection moulding or extrusion, in particular by extrusion blow moulding, coextrusion blow moulding or sequential blow moulding with and without 3D hose manipulation. For example, the polyamide moulding materials for the production of moulded articles have reduced surface carbonization in the moulded articles in subsequent long-term use at elevated temperatures. | 09-08-2011 |
| 20110039979 | FILLED POLYAMIDE MOLDING MATERIALS SHOWING A REDUCED WATER ABSORPTION - Filled polyamide molding materials, in particular polyamide molding materials with medium filler content, are producible from a polyamide blend and for example by compounding with chopped or endless fibers on two-screw extruders, and have a combination of reduced water absorption and good mechanical properties, which results in very good dimensional stability and reduced variation of the electrical properties of the produced molded part, such as an antenna housings of stationary or mobile communication devices. These thermoplastic polyamide molding materials are suitable for manufacturing molded parts and other semi-finished or finished parts, for example by extrusion, injection molding, pressing, direct process or direct compounding, respectively, wherein the compounded polyamide molding material is directly processed by injection molding or other shaping methods. | 02-17-2011 |
| 20100323185 | METALLICALLY COATED LIGHT-REFLECTING COMPONENTS BASED ON THERMOPLASTIC MOLDING COMPOUNDS - Relates to the use of a thermoplastic polymer molding compound for producing metallically coated light-reflecting components based on thermoplastics, which are suitable for operating temperatures of at least 200° C. The polymer molding compound used according to the present invention is characterized in that it comprises polyamides which are selected from a group which comprises homopolyamides, copolyamides, and mixtures (blends) made of homopolyamides and copolyamides and mixtures made of homopolyamides or copolyamides, these polyamides being selected from a group which comprises amorphous and transparent polyamides, and these polyamides having a glass transition temperature (Tg) of at least 205° C. Light-reflecting components produced according to the use according to the present invention are suitable for operating temperatures of at least 200° C. and comprise reflectors for traveling lights of vehicles, for signal and lighting devices, and reflectors for solar collectors. | 12-23-2010 |
| 20100028646 | POLYAMIDE MOLDING MATERIALS WITH AN IMPROVED FLOWABILITY, THE PRODUCTION THEREOF AND ITS USE - The invention relates to a housing from a polyamide moulding compound containing 70 to 99.5% by weight of at least one thermoplastic polyamide and 0.5 to 30% by weight of at least one polyamide oligomer with linear or branched chain structure with a number average molar mass of 800 to 5000 g/mol with basic end groups which are at least partially NH | 02-04-2010 |
| 20090131569 | Polyamide Molding Materials with an Improved Flowability, the Production Thereof and Its Use - The invention relates to a polyamide moulding compound containing 70 to 99.5% by weight of at least one thermoplastic polyamide and 0.5 to 30% by weight of at least one polyamide oligomer with linear or branched chain structure with a number average molar mass of 800 to 5000 g/mol with basic end groups which are at least partially NH | 05-21-2009 |
| 20080300347 | Adhesive Formulation, Method for Production and Use Thereof - The invention relates to an adhesive formulation for the treatment of reinforcing layers which are provided for the production of reinforced polymer products, the adhesive formulation containing dissolved epoxide. | 12-04-2008 |