Bormioli Luigi S.p.A. Patent applications |
Patent application number | Title | Published |
20150353416 | METHOD FOR INTERNALLY COATING A HOLLOW GLASS BODY - The present invention regards a method for internally coating a hollow glass body comprising the steps of: (a) applying on at least one internal surface of said hollow body at least one coating composition in form of liquid dispersion comprising at least one glass frit and at least one polymeric dispersing agent; (b) subjecting said internal surface comprising said coating composition to a thermal treatment, so as to obtain a vitrified coating layer. | 12-10-2015 |
20120214003 | PROCESS FOR APPLYING A SHATTERPROOF COATING TO THE SURFACE OF A GLASS ITEM - This invention relates to a process for applying a shatterproof coating to the surface of a glass item, comprising the following steps: (a) applying, on at least one portion of the surface of a glass item, a polymerisable composition comprising (i) a resin selected from the group consisting of polyurethane resins, polyester resins, acrylic resins, silicone resins and/or their mixes, in water or in an organic solvent; (ii) an adhesion promoter based on an organosilane compound; (iii) possibly a UV photo-initiator; (b) evaporating the water or the organic solvent; (c) polymerising said composition, forming on the glass item a shatterproof coating film capable of containing the dispersion of the glass fragments that may form in the event of the breakage of the item. The process also preferably comprises a step for the application of an additional anti-wear coating film on top of the shatterproof coating. | 08-23-2012 |
20120100329 | Article made from overmoulded composite material and relative preparation method - An article made from overmoulded composite material ( | 04-26-2012 |
20100203271 | PROCESS FOR INCREASING THE ABRASION RESISTANCE OF A PRE-DETERMINABLE PART OF THE SURFACE OF A GLASS CONTAINER - The present invention relates to a process for increasing the abrasion resistance of a pre-determinable part of the surface of an annealed glass container comprising the following operative phases: a) applying a liquid composition comprising an organo-titanate compound on a pre-determinable part of the annealed glass container surface by spraying at room temperature;
| 08-12-2010 |